MVR (300°C/1.2 kg) 19 cm³/10 min; low viscosity; easy release; flame retardant; variable content of filler for high reflectance application; injection molding
| Original Document | Technical Datasheet-ISO(English) Technical Datasheet-ISO(Chinese) | |||
| Features | Flame RetardantLight ReflectanceMold ReleaseLow viscosity | |||
| Processing | Injection | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | ***~*** g/cm³ | ISO 1183 | |
Melt Volume Flow Rate(MVR) | |||
300°C/1.2 kg | *** cm³/10 min | ISO 1133 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | ***~*** Mpa | ISO 527-1/-2 | 1 mm/min |
Tensile Strength | |||
Yield | *** Mpa | ISO 527-1/-2 | 5 mm/min |
Break | ***~*** Mpa | ISO 527-1/-2 | 5 mm/min |
Tensile Elongation | |||
Yield | *** % | ISO 527-1/-2 | 5 mm/min |
Break | ***~*** % | ISO 527-1/-2 | 5 mm/min |
Nominal Tensile Strain at Break | *** % | ISO 527-1/-2 | 5 mm/min |
Puncture | |||
Force | ***~*** N | ISO 6603-2 | 23℃ |
Energy | ***~*** J | ISO 6603-2 | 23℃ |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Unnotched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 180/A | Complete Break |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Vicat Softening Temperature(VST) | ***~*** °C | ISO 306 | 50 N; 50°C/h |
Relative Temperature Index(RTI), Imp | |||
1.5/1.6 mm | *** °C | UL 746B | |
Relative Temperature Index(RTI), Elec | |||
1.5/1.6 mm | *** °C | UL 746B | |
Relative Temperature Index(RTI), Str | |||
1.5/1.6 mm | *** °C | UL 746B | |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Flame Rating | |||
V-0 | *** mm | UL94 | WT |
| Optical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Reflectance | ***~*** % | JIS 8722 | 4 mm |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.