Miramid® DK2520CW is a Polyamide 6 (Nylon 6) material filled with 20% glass fiber and 25% mineral. It is available in Europe for injection molding.
Important attributes of Miramid® DK2520CW are:
Flame Rated
Chemical Resistant
Crystalline
Good Aesthetics
Good Dimensional Stability
Typical applications include:
Appliances
Engineering/Industrial Parts
| Original Document | Technical Datasheet-ISO(English) | |||
| Features | Dimensional StabilityChemical ResistanceFilled & Reinforced | |||
| Processing | Injection | |||
| Reinforced | 20% Glass Fiber25% Mineral45% Glass Fiber+Minal | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | Dry |
Water Absorption | *** % | ISO 62 | Dry |
Water Absorption | ***~*** % | ISO 62 | Dry |
Viscosity | *** cm³/g | ISO 307 | Dry |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-2 | Conditioned,23℃ |
Tensile Modulus | *** Mpa | ISO 527-2 | Dry,23℃ |
Tensile Strength | |||
Break | *** Mpa | ISO 527-2 | Conditioned,23℃ |
Break | *** Mpa | ISO 527-2 | Dry,23℃ |
Tensile Elongation | |||
Break | *** % | ISO 527-2 | Conditioned,23℃ |
Break | *** % | ISO 527-2 | Dry,23℃ |
Flexural Strength | |||
- | *** Mpa | ISO 178 | Conditioned,23℃ |
- | *** Mpa | ISO 178 | Dry,23℃ |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | Dry |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | Dry |
Charpy Unnotched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | Dry |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Dry |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Ball Indentation Hardness | *** Mpa | ISO 2039-1 | Dry |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-2 | Dry |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75-2 | Dry |
Melt Temperature(Tm) | *** °C | ISO 3146 | Dry |
Temperature at Short Circle Operation | *** °C | - | Dry |
Temperature index (TI)-Tensile Strength | |||
5000 h | *** °C | ISO 2578 | Dry |
20000 h | *** °C | ISO 2578 | Dry |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Flame Rating | |||
HB | *** mm | UL94 | Dry |
Glow Wire Flammability Index(GWFI) | |||
1mm | *** °C | IEC 60695-2-12 | Dry |
FMVSS | *** pass | FMVSS 302 | Dry |
| Electrical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Volume Resistivity | *** Ohm-cm | IEC 60093 | Conditioned |
Volume Resistivity | *** Ohm-cm | IEC 60093 | Dry |
Dielectric Constant(Permittivity) | |||
1MHz | *** - | IEC 60250 | Conditioned |
1MHz | *** - | IEC 60250 | Dry |
Dissipation Factor | |||
1MHz | *** E-4 | IEC 60250 | Conditioned |
1MHz | *** E-4 | IEC 60250 | Dry |
Comparative Tracking Index (CTI) | |||
- | *** V | IEC 60112 | Dry |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.