Torlon® 4203L

PAI(聚酰胺酰亚胺)

索尔维(苏威)(Solvay)

产品描述

Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals.

Torlon® 4203L resin offers outstanding electrical properties, which makes it ideal for high performance parts such as connectors, switches and relays. In addition Torlon® 4203L polyamide-imide can be used in applications such as thrust washers, spline liners, valve seats, bushings, bearings, wear rings, cams and other applications requiring strength at high temperature and resistance to wear.

  • High Flow: Torlon® 4203L-HF

  • Low Flow: Torlon® 4203L-LF

    基本信息
    原厂资料
    物性表(英文)
    产品特性
    耐疲劳
    高冲击
    耐热
    阻燃
    耐磨
    抗蠕变
    耐化学性
    颜色形状
    粒状
    成型方式
    注塑
    挤出
    型材挤出
    机加工
    法规认证
    RoHS(欧盟电子电气设备中有害物质)
    增强填充
    PTFE
    技术参数
    物理性能 值/单位 测试标准 测试条件

    比重

    1.42 - ASTM D792

    收缩率

    纵向(Flow)

    0.6~0.85 % ASTM D 955

    吸水率

    0.33 % ASTM D570
    24 hr
    机械性能 值/单位 测试标准 测试条件

    拉伸强度

    -

    152 Mpa ASTM D 638

    -

    192 Mpa ASTM D 1708

    拉伸延伸率

    断裂(brk)

    7.6 % ASTM D638

    断裂(brk)

    15 % ASTM D 1708

    弯曲强度

    -

    118 Mpa ASTM D790
    232℃

    -

    241 Mpa ASTM D790
    23℃

    弯曲模量

    3590 Mpa ASTM D790
    232℃

    弯曲模量

    5030 Mpa ASTM D790
    23℃

    拉伸模量

    4480 Mpa ASTM D638

    拉伸模量

    4900 Mpa ASTM D 1708

    泊松比

    0.45 - ASTM E 132

    压缩模量

    4000 Mpa ASTM D 695

    抗压强度

    221 Mpa ASTM D 695
    冲击性能 值/单位 测试标准 测试条件

    悬臂梁缺口(Izod Notched)

    -

    140 J/m ASTM D 256

    悬臂梁无缺口(Izod Unnotched)

    -

    1100 J/m ASTM D 4812
    热学性能 值/单位 测试标准 测试条件

    热变形温度(HDT)

    1.8 Mpa (264 psi)(18.6kg/cm²)

    278 °C ASTM D648
    Unannealed

    线性膨胀系数(CLTE)

    纵向(Flow)

    31 E-6 cm/cm/℃ ASTM E831

    玻璃化温度(Tg)

    277 °C ISO 11357-2

    导热系数

    0.26 W/(m K) ASTM C 177
    电学性能 值/单位 测试标准 测试条件

    体积电阻率

    2.0E+17 Ohm-cm ASTM D257

    表面电阻率

    5.0E+18 Ohm ASTM D257

    介电常数(DK)

    60 Hz

    4.2 - ASTM D 150

    1MHz

    3.9 - ASTM D 150

    耗散因数(DF)

    60 Hz

    260 E-4 ASTM D 150

    1MHz

    310 E-4 ASTM D150

    绝缘强度

    23 kV/mm ASTM D149

    此物性表中的信息由阿技材料库从该材料的生产商处获得。阿技材料库尽最大努力确保此数据的准确性。 但是阿技材料库对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。