TECHNYL® A 60G1 V30 Natural is a polyamide 66 based on a non-halogenated flame retardant system, reinforced with 30% of glass fiber, heat stabilized, for injection moulding. This grade offers excellent flame retardancy properties (UL 94, 5VA, GWIT) combined with excellent processing, mechanical and electrical performance. It can withstand temperatures of 160°C for over 6000 hours and has a UL F1 rating for weatherability resistance
| Original Document | Technical Datasheet(English) | |||
| Features | Flame RetardantFilled & Reinforced | |||
| Additive | Flame RetardantHeat Stabilizer | |||
| Appearance | Pellets/GranulesNatural ColorBlackGray Color | |||
| Processing | Injection | |||
| Compliance | EN 45545NF F 16-101REACH (EC 1907/2006)RoHSUL QMFZ2 | |||
| Reinforced | 30% Glass Fiber | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | Dry |
Mold Shrinkage | |||
Flow | *** % | ISO 294-4 | Dry |
Across Flow | *** % | ISO 294-4 | Dry |
Outdoor Suitability UL F1/F2 | |||
F1 | *** - | UL 746C | |
Water Absorption | *** % | ISO 62 | 24 hr, 23°C |
Water Absorption | *** % | ISO 62 | Equilibrium, 23°C, 50% RH |
Water Absorption | *** % | ISO 62 | Saturation, 23°C |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-2/1A | Conditioned,23℃ |
Tensile Modulus | *** Mpa | ISO 527-2/1A | Dry,23℃ |
Tensile Strength | |||
Break | *** Mpa | ASTM D638 | Conditioned,23℃ |
Break | *** Mpa | ASTM D638 | Dry,23℃ |
Break | *** Mpa | ISO 527-2/1A | Conditioned,23℃ |
Break | *** Mpa | ISO 527-2/1A | Dry,23℃ |
Tensile Elongation | |||
Break | *** % | ASTM D638 | Dry,23℃ |
Break | *** % | ISO 527-2 | Conditioned,23℃ |
Break | *** % | ISO 527-2 | Dry,23℃ |
Flexural Modulus | *** Mpa | ASTM D790 | Conditioned,23℃ |
Flexural Modulus | *** Mpa | ASTM D790 | Dry,23℃ |
Flexural Modulus | *** Mpa | ISO 178 | Conditioned,23℃ |
Flexural Modulus | *** Mpa | ISO 178 | Dry,23℃ |
Flexural Strength | |||
- | *** Mpa | ASTM D790 | Conditioned,23℃ |
- | *** Mpa | ASTM D790 | Dry,23℃ |
- | *** Mpa | ISO 178 | Conditioned,23℃ |
- | *** Mpa | ISO 178 | Dry,23℃ |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | Dry |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | Dry |
Charpy Unnotched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | Dry |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Dry |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** J/m | ASTM D256 | Dry |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75-2/Af | Dry,Annealed |
Melt Temperature(Tm) | *** °C | ISO 11357-3 | Dry |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Flame Rating | |||
V-0 | *** mm | UL94 | Dry |
V-0 | *** mm | UL94 | Dry |
V-0 | *** mm | UL94 | Dry |
5VA | *** mm | UL94 | Dry |
5VA | *** mm | UL94 | Dry |
Oxygen Index | *** % | ISO 4589 | Dry |
Glow Wire Flammability Index(GWFI) | |||
0.8mm | *** °C | IEC 60695-2-12 | Dry |
1.6mm | *** °C | IEC 60695-2-12 | Dry |
3.2mm | *** °C | IEC 60695-2-12 | Dry |
Glow Wire Ignition Test(GWIT) | |||
0.8mm | *** °C | IEC 60695-2-13 | Dry |
European Railways Certifications | *** HL | EN 45545-2 | |
European Railways Certifications | *** HL | EN 45545-2 | |
French Railways Certifications | *** - | NF F16-101 | French Fire Index |
French Railways Certifications | *** - | NF F16-101 | French Smoke Index |
| Electrical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Surface Resistivity | *** Ohm | IEC 60093 | Dry |
Comparative Tracking Index (CTI) | |||
Solution A | *** V | IEC 60112 | Dry |
Dielectric Strength | *** kV/mm | IEC 60243-1 | Dry,0.8mm |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.