Omnix® DW-4050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture absorption.
Omnix® DW-4050 is characterized by high stiffness and strength, very good impact properties, good dimensional stability and high flow properties. This material is an economical alternative for food service applications using die-cast alloys.
Omnix® DW-4050 is cleared for use under United States Food and Drug Administration (FDA) Conditions of Use B through H, in contact with all food types except Food Type VI C, Beverages containing more than 8 percent alcohol.
Omnix® DW-4050 is also cleared for food contact use by European Union regulations. For specific clearances, please contact your Solvay representative.
It processes readily using conventional injection molding machines and methods. Water-cooled molds are suitable for use with this grade.
Black: Omnix® DW-4050 BK 001
| Original Document | Technical Datasheet(English) | |||
| Features | High StrengthHigh Stiffness/RigidityHigh ImpactGood SurfaceDimensional StabilityFast Cycle TimeGood PaintablilityHigh FlowFilled & Reinforced | |||
| Appearance | Pellets/GranulesBlack | |||
| Processing | Injection | |||
| Compliance | ACSDVGW W270EU 2011/10/ECFDAKTWNSFRoHSWRAS | |||
| Reinforced | 50% Glass Fiber | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | Dry |
Mold Shrinkage | |||
Flow | *** % | ISO 294-4 | Dry |
Across Flow | *** % | ISO 294-4 | Dry |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-2 | Conditioned |
Tensile Modulus | *** Mpa | ISO 527-2 | Dry |
Tensile Strength | |||
Yield | *** Mpa | ISO 527-2 | Conditioned |
Yield | *** Mpa | ISO 527-2 | Dry |
Tensile Elongation | |||
Break | *** % | ISO 527-2 | Conditioned |
Break | *** % | ISO 527-2 | Dry |
Flexural Modulus | *** Mpa | ISO 178 | Dry |
Flexural Strength | |||
- | *** Mpa | ISO 178 | Dry |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179 | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179 | Dry |
Charpy Unnotched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179 | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179 | Dry |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 180 | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 180 | Dry |
Izod Unnotched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 180 | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 180 | Dry |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Melt Temperature(Tm) | *** °C | ISO 11357-3 | Dry |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.