AjiENG.com

Aji New Material (Qingdao) Co.,LTD

No.47 Huadingshan Road, Qingdao City, Shandong Province, China.
Tel: +86 532 86871530
Email: info@ajieng.com

Terluran® GP-35 White

ABS

INEOS Styrolution

Product Description
DESCRIPTION Terluran® GP-35 White is a new version of Terluran GP-35 containing a primary package of white pigments and UV stabilization. Just as GP-35 this new grade is suitable for self-coloring with the additional benefit to already contain a primar
General
Original Document
Technical Datasheet(English)
Features
High Impact
Heat Resistance
Good Surface
High Gloss
Good Coloring
UV Stabiltiy
High Flow
Processing
Injection
Specifications
Physical Value/Unit(Sign in to View) Test Standard Test Condition

Density/Specific Gravity

*** g/cm³ ISO 1183

Melt Volume Flow Rate(MVR)

220°C/10.0 kg

*** cm³/10 min ISO 1133

Mold Shrinkage

-

***~*** % ISO 294-4

Water Absorption

*** % ISO 62
Saturated at 23 °C

Moisture /Humidity Absorption

*** % ISO 62
Equilibrium 23 °C/50% RH
Mechanical Value/Unit(Sign in to View) Test Standard Test Condition

Tensile Modulus

*** Mpa ISO 527

Tensile Strength

Yield

*** Mpa ISO 527

Tensile Elongation

Yield

*** % ISO 527

Break

*** % ISO 527
min.

Nominal Tensile Strain at Break

*** % ISO 527

Flexural Strength

-

*** Mpa ISO 178
Impact Value/Unit(Sign in to View) Test Standard Test Condition

Charpy Notched Impact Strengh

-30℃ (-22℉)

*** kJ/m² ISO 179/1eA

23℃ (73℉)

*** kJ/m² ISO 179/1eA

Charpy Unnotched Impact Strengh

-30℃ (-22℉)

*** kJ/m² ISO 179/1eU

23℃ (73℉)

*** kJ/m² ISO 179/1eU

Izod Notched Impact Strengh

-30℃ (-22℉)

*** kJ/m² ISO 180/A

23℃ (73℉)

*** kJ/m² ISO 180/A
Hardness Value/Unit(Sign in to View) Test Standard Test Condition

Ball Indentation Hardness

*** Mpa ISO 2039-1
Thermal Value/Unit(Sign in to View) Test Standard Test Condition

Heat Deflection Temperature(HDT)

0.45 Mpa (66 psi)(4.6kg/cm²)

*** °C ISO 75
annealed 4 h/80 °C

1.8 Mpa (264 psi)(18.6kg/cm²)

*** °C ISO 75
annealed 4 h/80 °C

Vicat Softening Temperature(VST)

*** °C ISO 306
VST/A/50 (10N, 50 °C/h)

Vicat Softening Temperature(VST)

*** °C ISO 306
VST/B/50 (50N, 50 °C/h)

Coefficient of Linear Thermal Expansion

-

***~*** E-6/°C ISO 11359

Thermal Conductivity

*** W/(m K) DIN 52612-1

Processing Temperature

***~*** °C -

Mould temperature

***~*** °C -
Electrical Value/Unit(Sign in to View) Test Standard Test Condition

Volume Resistivity

*** Ohm-m IEC 60093
min.

The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.