Polyamide 6 (reinforced) Reinforced with glass fiber 30%, black color, heat stabilized
| Original Document | Technical Datasheet(English) | |||
| Features | Heat StabilizedFilled & Reinforced | |||
| Appearance | Black | |||
| Processing | Injection | |||
| Reinforced | 30% Glass Fiber | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Mold Shrinkage | |||
Flow | *** % | Internal | 30x100x3t |
Across Flow | *** % | Internal | 30x100x3t |
Water Absorption | *** % | - | 23℃/50%RH |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-1/-2 | |
Tensile Strength | |||
Yield | *** Mpa | ISO 527-1/-2 | |
Tensile Elongation | |||
Break | *** % | ISO 527-1/-2 | |
Flexural Modulus | *** Mpa | ISO 178 | |
Flexural Strength | |||
- | *** Mpa | ISO 178 | |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179-1/1eA | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Rockwell M | *** M | ISO 2039-2 | |
Rockwell R | *** R | ISO 2039-2 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-1/-2 | |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75-1/-2 | |
Coefficient of Linear Thermal Expansion | |||
- | *** E-6/°C | ISO 11359-2 | |
Melt Temperature(Tm) | ***~*** °C | ISO 11357 |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.