Luran ECO 368R is a general purpose grade of SAN with well-balanced properties, suitable for injection molding and extrusion. It features very good transparency, good heat resistance and very good dimensional stability. Luran ECO 368R BC70 is an ISCC compliant product leading to a substitution of fossil source styrene with ISCC certified bio-attributed styrene.
FEATURES
- Chemical resistance
- Heat resistance
- High surface quality
- Transparency
APPLICATIONS
- Water filters
- Mixers and blenders
- Food contact applications
- Cosmetic packaging
| Original Document | Technical Datasheet(English) | |||
| Resin ID | SAN | |||
| Features | Heat ResistanceHigh TransparencyGood SurfaceDimensional StabilityBio-basedFood ContactChemical Resistance | |||
| Applications | Cosmetics PackagingMixers and blendersWater Filters | |||
| Processing | InjectionExtrusion | |||
| Compliance | ISCC PLUS | |||
| Diagrams | Viscosity-shear rateShearstress-shear rateStress-strainSecant modulus-strainStress-strain (isochronous)(Creep) 23°CCreep modulus-time 23°CSpecific volume-temperature (pvT)Tensile modulus-temperature | |||
| Biobased/Renewable | 70% Yes | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Melt Volume Flow Rate(MVR) | |||
220°C/10.0 kg | *** cm³/10 min | ISO 1133 | |
Mold Shrinkage | |||
- | ***~*** % | ISO 294-4 | |
Moisture /Humidity Absorption | *** % | ISO 62 | Equilibrium 23 °C/50% RH |
Post Consumer Recycled | *** % | Internal | min. |
Carbon Footprint Reduction | *** % | ISO 14044 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527 | |
Tensile Strength | |||
Yield | *** Mpa | ISO 527 | 23 °C |
Tensile Elongation | |||
Break | *** % | ISO 527 | 23 °C |
Flexural Modulus | *** Mpa | ISO 178 | |
Flexural Strength | |||
- | *** Mpa | ISO 178 | 23 °C |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | |
Charpy Unnotched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 180/A | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Ball Indentation Hardness | *** Mpa | ISO 2039-1 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75 | annealed 4 h/80 °C |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75 | annealed 4 h/80 °C |
Vicat Softening Temperature(VST) | *** °C | ISO 306 | VST/B/50 (50N, 50 °C/h) |
Coefficient of Linear Thermal Expansion | |||
- | *** E-6/°C | ISO 11359 | |
Thermal Conductivity | *** W/(m K) | ISO 22007 | |
Processing Temperature | ***~*** °C | - | |
Mould temperature | ***~*** °C | - | |
| Optical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Light Transmission | *** % | ASTM D1003 | at 550 nm |
Haze | *** % | ASTM D1003 | |
Refractive Index | *** - | ISO 489 | Sodium D Line |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.