Glass-fiber reinforced, heat aging resistant and laser-markable injection molding grade based on semi-crystalline polyamides with partially aromatic content. The product can be characterized as compound with very high strength and stiffness even after moisture uptake.
Markets & applications
- Automotive: structural parts, metal replacement, brake parts, interior, powertrain
- E&E: electrical appliances, cell phones
- Consumer goods: home appliances, consumer electronics, furniture fittings
| Original Document | Technical Datasheet(English) | |||
| Resin ID | PA*-GF40 | |||
| Availability | AsiaEuropeNorth AmericaMiddle EastAfricaSouth & Central America | |||
| Features | High StrengthHigh Stiffness/RigidityGood Heat AgingLaser MarkableFilled & Reinforced | |||
| Applications | Electronics & Electrical ApplicationsHome appliancesStructural partsFurnitureCell PhonesMetal replacementAutomotive Interior PartsPowertrain Components | |||
| Appearance | Pellets/GranulesBlack | |||
| Processing | Injection | |||
| Diagrams | Viscosity-shear rateShearstress-shear rateStress-strainStress-strain (Cond.)Secant modulus-strainSecant modulus-strain (Cond.)Tensile modulus-temperatureTensile modulus-temperature (cond.) | |||
| Reinforced | 40% Glass Fiber | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Melt Volume Flow Rate(MVR) | |||
275°C/5 kg | *** cm³/10 min | ISO 1133 | |
Mold Shrinkage | |||
Flow | *** % | ISO 294-4, 2577 | |
Across Flow | *** % | ISO 294-4, 2577 | |
Moisture /Humidity Absorption | *** % | ISO 62 | |
Viscosity | *** cm³/g | ISO 307, 1157, 1628 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-1/-2 | Cond. |
Tensile Modulus | *** Mpa | ISO 527-1/-2 | Dry |
Tensile Strength | |||
Break | *** Mpa | ISO 527-1/-2 | Cond. |
Break | *** Mpa | ISO 527-1/-2 | Dry |
Tensile Elongation | |||
Break | *** % | ISO 527-1/-2 | Cond. |
Break | *** % | ISO 527-1/-2 | Dry |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | Cond. |
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | Cond. |
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | Dry |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | Dry |
Charpy Unnotched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | Cond. |
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | Dry |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Cond. |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Dry |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-1/-2 | |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75-1/-2 | |
Melt Temperature(Tm) | *** °C | ISO 11357-1/-3 |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.