medium viscosity; easy release; UV stabilized; UV 400 cut off; optical lenses
| Original Document | Technical Datasheet(English) Technical Datasheet(Chinese) | |||
| Features | Mold ReleaseUV StabiltiyMedium viscosity | |||
| Additive | UV-Stabilizer | |||
| Applications | Optical Lenses | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Melt Volume Flow Rate(MVR) | |||
300°C/1.2 kg | *** cm³/10 min | ISO 1133 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-1/-2 | 1 mm/min |
Tensile Strength | |||
Yield | *** Mpa | ISO 527-1/-2 | 5 mm/min |
Break | *** Mpa | ISO 527-1/-2 | 5 mm/min |
Tensile Elongation | |||
Yield | *** % | ISO 527-1/-2 | 5 mm/min |
Nominal Tensile Strain at Break | *** % | ISO 527-1/-2 | 5 mm/min |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Unnotched Impact Strengh | |||
-20℃ (-4℉) | *** kJ/m² | ISO 179/1eU | |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 21305 | |
| Optical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Light Transmission | *** % | ISO 13468-2 | 4 mm |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.