Finalloy SMV-66HM is a 15% mineral-filled and impact-modified polypropylene-based compound that combines a good impact-rigidity balance with very good processability. This material has been optimised to meet extremely severe specifications for low HC-emissions and odour in the car interior.
Finalloy SMV-66HM is UV and heat stabilised and is particularly suitable for the injection moulding of non-painted, visible automotive interior parts.
| Original Document | Technical Datasheet(English) | |||
| Features | Toughened/Impact ModifiedHeat StabilizedEasy processingLow OdorLow HC EmissionUV StabiltiyFilled & Reinforced | |||
| Additive | UV-StabilizerImpact ModifierHeat Stabilizer | |||
| Applications | Automotive Interior Trims | |||
| Processing | Injection | |||
| Reinforced | 15% Mineral | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Melt Mass Flow Rate(MFR) | |||
230°C/2.16 kg | *** g/10min | ISO 1133 | |
Mold Shrinkage | |||
Flow | ***~*** % | Internal | t=3mm |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527 | |
Tensile Strength | |||
Yield | *** Mpa | ISO 527 | |
Tensile Elongation | |||
Yield | *** % | ISO 527 | |
Break | *** % | ISO 527 | |
Flexural Modulus | *** Mpa | ISO 178 | |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | |
-20℃ (-4℉) | *** kJ/m² | ISO 179/1eA | |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore D hardness | *** D | ISO 868 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-2 | 120°C per hour |
Coefficient of Linear Thermal Expansion | |||
- | *** E-6/K | ISO 11359-2 | |
Melt Temperature(Tm) | ***~*** °C | Internal |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.