LNP THERMOCOMP Z1C00VI compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing proprietary fillers. Added features of this grade include: Ultra-Low Dielectric Constant and Loss Tangent for Laser Direct Structuring (LDS), High HDT, Low Warpage, Excellent Surface Finishing and Chemical Resistant.
| Original Document | Technical Datasheet(English) | |||
| Features | Heat ResistanceLow DielectricGood SurfaceLow WarpageLaser Direct StructuringChemical ResistanceFilled & Reinforced | |||
| Processing | Injection | |||
| Reinforced | Filler | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Mold Shrinkage | |||
Flow | ***~*** % | Internal | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ASTM D638 | 50 mm/min |
Tensile Modulus | *** Mpa | ISO 527 | 1 mm/min |
Tensile Strength | |||
Yield | *** Mpa | ASTM D638 | Type I, 50 mm/min |
Yield | *** Mpa | ISO 527 | 50 mm/min |
Break | *** Mpa | ISO 527 | 50 mm/min |
Break | *** Mpa | ASTM D638 | Type I, 50 mm/min |
Tensile Elongation | |||
Yield | *** % | ASTM D638 | Type I, 50 mm/min |
Yield | *** % | ISO 527 | 50 mm/min |
Break | *** % | ASTM D638 | Type I, 50 mm/min |
Break | *** % | ISO 527 | 50 mm/min |
Flexural Modulus | *** Mpa | ASTM D790 | 1.3 mm/min, 50 mm span |
Flexural Modulus | *** Mpa | ISO 178 | 2 mm/min |
Flexural Strength | |||
Break | *** Mpa | ASTM D790 | 1.3 mm/min, 50 mm span |
Break | *** Mpa | ISO 178 | 2 mm/min |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** J/m | ASTM D256 | |
23℃ (73℉) | *** kJ/m² | ISO 180/1A | 80*10*4 |
Izod Unnotched Impact Strengh | |||
23℃ (73℉) | *** J/m | ASTM D4812 | |
23℃ (73℉) | *** kJ/m² | ISO 180/1U | 80*10*4 |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm |
| Electrical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Dielectric Constant(Permittivity) | |||
1.1 GHz | *** - | Internal | |
1.9 GHz | *** - | Internal | |
10 GHz | *** - | Internal | |
Dissipation Factor | |||
1.1 GHz | *** E-4 | Internal | |
1.9 GHz | *** E-4 | Internal | |
10 GHz | *** E-4 | Internal |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.