FLEX NORYL WCA875 resin is a flexible, non-reinforced extrudable blend of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE). This material contains non-halogenated flame retardant and performance capable of meeting UL VW-1 requirements, 105C end use temperature rating, and heat deformation performance as defined by UL 1581. FLEX NORYL WCA875 resin is intended for evaluation in wire insulation applications in dark colors. It has a Shore A Hardness reading of 87 and exhibits superior thermal stability, very low water absorption, good electric properties, and low specific gravity. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.
| Original Document | Technical Datasheet(English) | |||
| Features | DuctileHeat StabilizedFlame RetardantHalogen FreeCl- FreeBr- FreeInsulatingDimensional StabilityLow WarpageEasy processingHydrolysis ResistanceLow DensityLow Moisture Absorption | |||
| Processing | ExtrusionWire & Cable Extrusion | |||
| Compliance | UL VW-1 | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Melt Mass Flow Rate(MFR) | |||
250°C/10.0 kg | *** g/10 min | ASTM D 1238 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Break | *** Mpa | ISO 527 | 50 mm/min |
Break | *** Mpa | ASTM D638 | Type I, 50 mm/min |
Tensile Elongation | |||
Break | *** % | ASTM D638 | Type I, 50 mm/min |
Break | *** % | ISO 527 | 50 mm/min |
Flexural Modulus | *** Mpa | ASTM D790 | 12.5 mm/min, 100 mm span |
Flexural Modulus | *** Mpa | ISO 178 | 12.5 mm/min |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Brittleness Temperature | *** °C | ASTM D 746 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore A hardness | *** A | ASTM D 2240 | 30S reading |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Oxygen Index | *** % | ISO 4589 | |
Glow Wire Flammability Index(GWFI) | |||
3mm | *** °C | IEC 60695-2-12 | pass |
Glow Wire Ignition Test(GWIT) | |||
3.0mm | *** °C | IEC 60695-2-13 | |
NBS Smoke Density | *** - | ASTM E 662 | on 0.5mm plaque, Flame, Ds, max |
NBS Smoke Density | *** - | ASTM E 662 | on 0.5mm plaque, Non-flame, Ds, max |
| Electrical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Volume Resistivity | *** Ohm-cm | ASTM D257 | |
Dielectric Constant(Permittivity) | |||
1MHz | *** - | IEC 60250 | |
Dissipation Factor | |||
1MHz | *** E-4 | IEC 60250 | |
Comparative Tracking Index (CTI) | |||
- | *** V | IEC 60112 | |
Dielectric Strength | *** kV/mm | IEC 60243-1 | in oil, 2.0mm |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.