Sarlink® TPV is a global brand of thermoplastic vulcanizate, an innovative material with the properties of a rubber that can be processed as a plastic. Sarlink offers time-tested TPV expertise, an extensive product range, superior customer service and fully colorable, high-performance solutions for many complex application challenges.
3000 series Highly crosslinked EPDM grade
Features: Excel in molding, appearance, and flexure fatigue resistance.
| Original Document | Technical Datasheet(English) | |||
| Processing | InjectionExtrusion | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Mold Shrinkage | |||
Flow | *** % | Internal | 3mm thickness |
Across Flow | *** % | Internal | 3mm thickness |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
- | *** Mpa | ASTM D 412 | Cross direction |
- | *** Mpa | ASTM D 412 | Flow direction |
at 100% strain | *** Mpa | ASTM D 412 | Cross direction |
at 100% strain | *** Mpa | ASTM D 412 | Flow direction |
Tensile Elongation | |||
Break | *** % | ASTM D 412 | Cross direction |
Break | *** % | ASTM D 412 | Flow direction |
Tear Strength | *** kN/m | ASTM D 624 | Unnicked, Cross direction |
Compression Set | *** % | ASTM D 395 | 125℃, 70Hrs |
Compression Set | *** % | ASTM D 395 | 23℃, 22Hrs |
Compression Set | *** % | ASTM D 395 | 70℃, 22Hrs |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Brittleness Temperature | *** °C | ISO 812 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore A hardness | *** A | ASTM D 2240 | 5sec, Extruded sample |
Shore A hardness | *** A | ASTM D 2240 | 5sec, Injection molded sample |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Flame Rating | |||
HB | *** mm | UL94 | |
| Aging | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Hardness(Heat Aging) | *** - | ASTM D573 | Change, 135℃, 1000Hrs |
Hardness(Heat Aging) | *** - | ASTM D573 | Change, 150℃, 168Hrs |
Tensile Strength(Heat Aging) | *** % | ASTM D573 | Retention, 135℃, 1000Hrs |
Tensile Strength(Heat Aging) | *** % | ASTM D573 | Retention, 150℃, 168Hrs |
Elonggation(Heat Aging) | *** % | ASTM D573 | Retention, 135℃, 1000Hrs |
Elonggation(Heat Aging) | *** % | ASTM D573 | Retention, 150℃, 168Hrs |
Change in Volume | *** % | ASTM D471 | ASTM Oil#3, 125℃, 70Hrs |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.