Heat-resistant PP compounds are products that outperform the competition. The addition of talc as an inorganic filler to homo-polypropylene provides for enhanced strength and heat-resistance. These products have a variety of base PPs, such as HIPP (High Isotactic or High crystalline Polypropylene), and are manufactured with special Hanwha Total processing technology for high quality and customer satisfaction. These grades feature superior rigidity, long-term heat resistance, anti-static property, as well as dimensional stability.
Practical applications include use in electric and electronic product parts and household appliances.
Characteristics
▶ High heat-resistance and dimensional stability due to use of talc as an inorganic filler;
▶ Superior strength ;
▶ Superior processability;
▶ Superior long-term heat-resistance, and anti-static property.
Applications
▶ Electric and electronic product exteriors, - Dish washers and dish dryers; - Coffee maker parts and microwave ovens;
▶ Household appliance and industrial products, - Food containers, outdoor chairs, outdoor tables.
| Original Document | Technical Datasheet(English) | |||
| Features | Heat ResistanceHeat StabilizedDimensional StabilityFilled & Reinforced | |||
| Reinforced | Talc | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D 1505 | |
Melt Mass Flow Rate(MFR) | |||
230°C/2.16 kg | *** g/10min | ASTM D 1238 | |
Mold Shrinkage | |||
- | ***~*** % | Internal | 2mm(t) |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** kg/cm² | ASTM D638 | 50mm/min |
Tensile Elongation | |||
Break | *** % | ASTM D638 | 50mm/min |
Flexural Modulus | *** kg/cm² | ASTM D790 | 5mm/min |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** kg·cm/cm | ASTM D256 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Rockwell R | *** R | ASTM D785 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ASTM D648 |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.