Toughened PP
Key feature:
High flowability; High impact; High rigidity
Application:
Special materials for Thin-walled injection molding; Bumper
| Original Document | Technical Datasheet(Chinese&English) | |||
| Features | High ImpactToughened/Impact ModifiedHigh Flow | |||
| Reinforced | 25% Filler | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Melt Mass Flow Rate(MFR) | |||
230°C/2.16 kg | *** g/10min | ISO 1133 | |
Mold Shrinkage | |||
Flow | *** % | ISO 294 | |
Across Flow | *** % | ISO 294 | |
Filled/Ash | *** % | ISO 1172 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Break | *** Mpa | ISO 527 | 50mm/min |
Tensile Elongation | |||
Break | *** % | ISO 527 | 50mm/min |
Flexural Modulus | *** Mpa | ISO 178 | 2mm/min |
Flexural Strength | |||
- | *** Mpa | ISO 178 | 2mm/min |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Unnotched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179 | |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 180 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-2 | |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Burning Rate | *** mm/min | ISO 1210 | Horizontal burning rate |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.