Vistamaxx 7020BF is a semi-crystalline copolymer of propylene and ethylene produced using ExxonMobil’s proprietary metallocene catalyst technology. It has excellent elastomeric properties, is easy to process , and is compatible with a wide variety of materials.
Key Features
• Improved color stability in polypropylene blends for nonwoven fabrics.
• Excellent adhesion to conventional or metallocene PP and PE.
• Very good elasticity and toughness.
• Particularly good for thermoplastic and polyolefinic blends where a balance of flexibility, transparency and impact performance is required.
| Original Document | Technical Datasheet(English) Technical Datasheet(Chinese) | |||
| Appearance | Pellets/Granules | |||
| Processing | Compounding | |||
| Compliance | RoHS | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | Internal | |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ASTM D1238 | |
230°C/2.16 kg | *** g/10min | Internal | |
Ethylene Content | *** % | Internal | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Break | *** Mpa | Internal | |
at 100% strain | *** Mpa | Internal | |
at 300% strain | *** Mpa | Internal | |
Tensile Elongation | |||
Break | *** % | Internal | |
Flexural Modulus | *** Mpa | Internal | 1% Secant |
Tear Strength | *** kN/m | Internal | Die C |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Vicat Softening Temperature(VST) | *** °C | Internal |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.