A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applications. This grade of Geolast TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and recyclable within the manufacturing stream.
Key Features
• Recyclable.
• Designed for improved fluid resistance.
| Original Document | Technical Datasheet(English) Technical Datasheet(Chinese) | |||
| Features | Good Heat AgingOil ResistantSoft | |||
| Appearance | Pellets/GranulesBlack | |||
| Processing | InjectionExtrusionSheet ExtrusionProfile ExtrusionBlow MoldingInjection Blow MoldingExtrusion Blow Molding | |||
| Compliance | RoHS | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Break | *** Mpa | ASTM D 412 | Across Flow, 23°C |
Break | *** Mpa | ISO 37 | Across Flow, 23°C |
at 100% strain | *** Mpa | ASTM D 412 | Across Flow, 23°C |
at 100% strain | *** Mpa | ISO 37 | Across Flow, 23°C |
Tensile Elongation | |||
Break | *** % | ASTM D 412 | Across Flow, 23°C |
Break | *** % | ISO 37 | Across Flow, 23°C |
Compression Set | *** % | ASTM D 395 | 125°C, 70 hr, Type 1 |
Compression Set | *** % | ASTM D 395 | 70°C, 22 hr, Type 1 |
Compression Set | *** % | ISO 815 | 125°C, 70 hr, Type A |
Compression Set | *** % | ISO 815 | 70°C, 22 hr, Type A |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Brittleness Temperature | *** °C | ASTM D 746 | |
Brittleness Temperature | *** °C | ISO 812 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore A hardness | *** A | ISO 868 | 15 sec, 23°C |
| Aging | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Hardness(Heat Aging) | *** % | ISO 188 | Change, in Air, 125°C, 168 hr |
Hardness(Heat Aging) | *** % | ASTM D573 | Change, in Air, 125°C, 168 hr |
Tensile Strength(Heat Aging) | *** % | ISO 188 | Change, in Air, 125°C, 168 hr |
Tensile Strength(Heat Aging) | *** % | ASTM D573 | Change, in Air, 125°C, 168 hr |
Elonggation(Heat Aging) | *** % | ISO 188 | Change, in Air, 125°C, 168 hr |
Elonggation(Heat Aging) | *** % | ASTM D573 | Change, in Air, 125°C, 168 hr |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.