ExxonMobil™ HD 7960.13 is a high molecular weight high density polyethylene blown film resin. Films made from HD 7960.13 resin exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 resin is particularly recommended for films less than 0.5 mil in thickness.
| Original Document | Technical Datasheet(English) Technical Datasheet(Chinese) | |||
| Additive | Heat StabilizerProcessing Aid | |||
| Appearance | Pellets/Granules | |||
| Processing | Film ExtrusionBlown Film | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D 1505 | |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ASTM D1238 | |
190℃/21.6 kg | *** g/10 min | ASTM D 1238 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Melt Temperature(Tm) | *** °C | Internal | Peak |
| Film | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ASTM D 882 | MD |
Yield | *** Mpa | ASTM D 882 | TD |
Break | *** Mpa | ASTM D 882 | MD |
Break | *** Mpa | ASTM D 882 | TD |
Tensile Elongation | |||
Break | *** % | ASTM D 882 | MD |
Break | *** % | ASTM D 882 | TD |
Elmondorf Tear | *** g | ASTM D 1922 | MD |
Elmondorf Tear | *** g | ASTM D 1922 | TD |
Secant Modulus | *** Mpa | ASTM D 882 | 1% Secant, MD |
Secant Modulus | *** Mpa | ASTM D 882 | 1% Secant, TD |
Dart Drop Impact | *** g | ASTM D 1709 |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.