UNIVAL™ DMDF-6230 NT High Density Polyethylene (HDPE) Resin is specifically designed for use in either intermittent or continuous blow molding equipment to produce containers up to 20 gallons in size -applications that require the combination of outstanding environmental stress crack resistance (ESCR) and, high impact strength. UNIVAL DMDF- 6230 NT HDPE resin is also considered a multipurpose blow molding resin designed for the high speed production of blow molded containers used for packaging household industrial chemicals (e.g., detergents, bleach, fabric softeners), toiletries and cosmetics (e.g., shampoos, creams, lotions, etc.), health and medicinal aids. In addition, it can be blow molded into other thin walled parts and houseware items, and also can be extruded into profiles or sheets.
Outstanding environmental stress crack resistance
High impact strength
Good extrusion characteristics
Formulated with a non-food grade antistatic agent
Complies with:
U.S. FDA 21 CFR 175.105
Consult the regulations for complete details.
| Original Document | Technical Datasheet(English) | |||
| Processing | Blow Molding | |||
| Compliance | FDA | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ASTM D1238 | |
190℃/21.6 kg | *** g/10 min | ASTM D 1238 | |
Environmental Stress Cracking Resistance | *** Hours | ASTM D 1693 | 50°C, 100% Igepal, F50 |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ASTM D638 | |
Break | *** Mpa | ASTM D638 | |
Tensile Elongation | |||
Yield | *** % | ASTM D638 | |
Break | *** % | ASTM D638 | |
Flexural Modulus | *** Mpa | ASTM D790 | 2% Secant |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Impact | *** kJ/m² | ASTM D 1822 | Type S |
Brittleness Temperature | *** °C | ASTM D 746 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore D hardness | *** D | ASTM D 2240 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ASTM D648 | Unannealed |
Vicat Softening Temperature(VST) | *** °C | ASTM D1525 | |
Melt Temperature(Tm) | *** °C | Internal | DSC |
Freezing temperature | *** °C | Internal | DSC |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.