Dow LDPE 5004I is used for fresh milk cartons, liquid/juice containers, dry foods packaging, snack foods packaging, moist foods packaging, and medical packaging. Dow LDPE extrusion coating resins provide optimal neck-in and draw-down performance with minimal taste/odor contribution.
A low melt index coating resin for demanding packaging applications
Complies with:
U.S. FDA 21 CFR 177.1520 (c) 2.2
U.S. FDA -DMF
Canadian HPFB No Objection (With Limitations)
EU, No 10/2011
Japan Hygienic Olefin and Styrene Plastics Association
Consult the regulations for complete details.
| Original Document | Technical Datasheet-ASTM(English) | |||
| Processing | Cast FilmExtrusion Coating | |||
| Compliance | Drug Master FileEU 2011/10/ECFDAHPFB (Canada)JHOSPA | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Density/Specific Gravity | *** g/cm³ | Internal | Base Density |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ASTM D1238 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Coefficient of Friction | *** - | ASTM 1894 | vs. Itself - Dynamic, Extrusion Coating |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Vicat Softening Temperature(VST) | *** °C | ASTM D1525 | |
Melt Temperature(Tm) | *** °C | Internal | DSC |
Processing Temperature | ***~*** °C | - | Melt Temperature |
| Optical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Haze | *** % | ASTM D1003 | 25.4 µm, Cast Film |
Gloss | *** - | ASTM D 2457 | 45°, 25.4 µm, Cast Film |
| Film | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ASTM D 882 | MD, 25 µm, Cast Film |
Yield | *** Mpa | ASTM D 882 | TD, 25 µm, Cast Film |
Break | *** Mpa | ASTM D 882 | MD, 25 µm, Cast Film |
Break | *** Mpa | ASTM D 882 | TD, 25 µm, Cast Film |
Tensile Elongation | |||
Break | *** % | ASTM D 882 | MD, 25 µm, Cast Film |
Break | *** % | ASTM D 882 | TD, 25 µm, Cast Film |
Puncture resistance | *** J/cm³ | Internal | 25 µm |
Film Toughness | *** J/cm³ | ASTM D882 | MD, 25 µm, Cast Film |
Film Toughness | *** J/cm³ | ASTM D882 | TD, 25 µm, Cast Film |
Elmondorf Tear | *** g | ASTM D 1922 | MD, 25 µm, Cast Film |
Elmondorf Tear | *** g | ASTM D 1922 | TD, 25 µm, Cast Film |
Dart Drop Impact | *** g | ASTM D 1709 | 25 µm, Cast Film |
Water Vapor Transmission Rate | *** g.mm/m².24hr | ASTM F 1249 | 25 µm, Extrusion Coating |
Seal Initiation Temperature | *** ℃ | Internal | 25 µm, Extrusion Coating |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.