DOWLEX™ 2750ST Polyethylene Resin is suitable for the production of high modulus blown and cast films. The resin offers an excellent balance of tensiles, tear and impact strength with good optics, and can be used to enable the reduction in gauge of various film structures.
Applications:
Various industrial, consumer and specialty films.
Complies with:
EU, No 10/2011
Consult the regulations for complete details.
| Original Document | Technical Datasheet(English) | |||
| Processing | Cast FilmBlown Film | |||
| Compliance | EU 2011/10/EC | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Density/Specific Gravity | *** g/cm³ | Internal | Base Density |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ASTM D1238 | |
| Film | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ASTM D 882 | MD, 50 µm |
Yield | *** Mpa | ASTM D 882 | TD, 50 µm |
Break | *** Mpa | ASTM D 882 | MD, 50 µm |
Break | *** Mpa | ASTM D 882 | TD, 50 µm |
Tensile Elongation | |||
Break | *** % | ASTM D 882 | MD, 50 µm |
Break | *** % | ASTM D 882 | TD, 50 µm |
Piercing strength | *** N | Internal | 50 µm |
Puncture resistance | *** J/cm³ | Internal | 50 µm |
Puncture resistance | *** J | Internal | 50 µm |
Elmondorf Tear | *** g | ASTM D 1922 | MD, 50 µm |
Elmondorf Tear | *** g | ASTM D 1922 | TD, 50 µm |
Secant Modulus | *** Mpa | ASTM D 882 | 2% Secant, MD, 50 µm |
Dart Drop Impact | *** g | ASTM D 1709 | 50 µm |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.