AXELERON™ CS O-3364 NT CPD is a high molecular weight, high-density polyethylene insulation compound ("CPD") providing excellent oxidative stability, toughness and abrasion resistance. AXELERON™ CS O-3364 NT CPD also provides excellent processing capability in high speed insulating extrusion processes. The AXELERON™ CS O-3364 NT CPD insulation compound has been optimized to yield increased insulation to conductor adhesion. The increased conductor adhesion improves processing latitude and insulation shrinkback performance for heavy wall insulation and tight pair twisting applications such as data grade LAN.
AXELERON™ CS O-3364 NT CPD provides good performance across the full range of twisted pair telecommunication insulation applications. AXELERON™ CS O-3364 NT CPD readily meets Telcordia and ICEA requirements as well as most international age testing standards and specifications for both solid and foam/skin telephone cable insulation use. In the demanding grease filled cable application, AXELERON™ CS O-3364 NT CPD provides superior long term aging performance meeting the stringent Telcordia testing requirements.
SPECIFICATIONS
AXELERON™ CS O-3364 NT CPD meets the following material specifications:
ASTM D 1248 Type III Category A-4, Grade E8 and E9
Federal LP-390 C, II-H, Grades 1 and 2, Category 4
Telephone wire insulated with AXELERON™ CS O-3364 NT CPD, using sound cable design and fabrication practices, will meet the following specifications:
Telcordia GR-421-CORE, Issue 1, December 1998, "Generic Requirements for Metallic Telecommunications Cables"
ICEA S-84-608, "Telecommunications Cable; Filled, Polyolefin Insulated, Copper Conductor -Technical Requirements"
REA PE 39, "Filled Telephone Cable"
REA PE 89, "Filled Telephone Cable with Expanded Insulation"
| Original Document | Technical Datasheet-ASTM(English) | |||
| Processing | Wire & Cable Extrusion | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ASTM D1238 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
- | *** Mpa | ASTM D 638 | |
Tensile Elongation | |||
Yield | *** % | ASTM D638 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Thermal Stress Crack Resistance | *** Hours | ASTM D2951 | |
| Electrical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Volume Resistivity | *** Ohm-cm | ASTM D257 | |
Dielectric Constant(Permittivity) | |||
1MHz | *** - | ASTM D1531 | |
Dissipation Factor | |||
1MHz | *** E-4 | ASTM D1531 | |
| Additional Information | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Oxidative Induction Time | *** Min | ASTM D4565 | 200°C |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.