ATTANE™ 4607GC Ultra Low Density Ethylene/Hexene Copolymer is a skin layer in cast film offers excellent low temperature hot tack properties combined with outstanding tear and impact strength. In stretch film applications, ATTANE™ 4607GC Ultra Low Density Ethylene/Hexene Copolymer exhibits excellent stretchability as well as good physical and cling properties. ATTANE™ 4607GC Ultra Low Density Ethylene/Hexene Copolymer can also be utilised in blown film coextrusion where it is combined with other resins having excellent bubble stability allowing ATTANE™ 4607GC Ultra Low Density Ethylene/Hexene Copolymer to be used as a sealant in multilayer film structures.
Applications:
Cling layer in cast stretch film.
Sealants in cast and blown films.
Complies with:
EU, No 10/2011- U.S. FDA FCN 741
Consult the regulations for complete details
| Original Document | Technical Datasheet(English) | |||
| Processing | Cast FilmBlown Film | |||
| Compliance | EU 2011/10/ECFDA | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Density/Specific Gravity | *** g/cm³ | Internal | Base Density |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ISO 1133 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Vicat Softening Temperature(VST) | *** °C | ASTM D1525 | |
Processing Temperature | ***~*** °C | - | Extrusion |
| Optical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Haze | *** % | ASTM D1003 | 23.0 µm |
Gloss | *** - | ASTM D 2457 | 45°, 23.0 µm |
| Film | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ISO 527-3 | MD, 23 µm |
Yield | *** Mpa | ISO 527-3 | TD, 23 µm |
Break | *** Mpa | ISO 527-3 | MD, 23 µm |
Break | *** Mpa | ISO 527-3 | TD, 23 µm |
Tensile Elongation | |||
Break | *** % | ISO 527-3 | MD, 23 µm |
Break | *** % | ISO 527-3 | TD, 23 µm |
Piercing strength | *** N | Internal | 23 µm |
Puncture resistance | *** J | Internal | 23 µm |
Elmondorf Tear | *** g | ASTM D 1922 | MD, 23 µm |
Elmondorf Tear | *** g | ASTM D 1922 | TD, 23 µm |
Dart Drop Impact | *** g | ISO 7765-1 | 23 µm |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.