Bormed HJ875MO is a resin intended for evaluation for use in Healthcare applications.
Bormed HJ875MO is a high flow polypropylene Homopolymer. High flow enables lower cycle time, high injection rate and design of thin wall packaging. This grade is formulated for optimised extractables. Material can be sterilised with vapour (121 °C for 20 minutes) or EtO.
Applications
Bormed HJ875MO has been evaluated according to different regulations and norms. Typical applications are mentioned below for Medical devices or Pharmaceutical & Diagnostic packaging. However, Borealis should be consulted for final approval to evaluate the use of Bormed HJ875MO .
Pipette tips Laboratory disposable Dosing units Aerosol devices Caps and closures Pharmaceutical & diagnostic packaging in solid dose form or for oral and/or topical admistration Bottles & Boxes as Packaging for pharmaceutical & diagnostic products
This grade may only be used for the applications listed in the Product Datasheet and only to the extent that the application is within the scope of the tests set out in the Statement on Compliance to Regulations on Medical Use for that grade. If an application is not listed in the Product Datasheet, the grade can be used for such application only after express written consent of the Borealis Marketing Manager, Healthcare. Borealis prohibits the use of any healthcare grade product in an implantable device that is introduced into the human body by surgical intervention and that is intended to remain in place following surgical procedure.
Special features
High flow Low extractables
| Original Document | Technical Datasheet-ISO(English) | |||
| Features | Fast Cycle TimeMedical Application/Health CareEtO sterilizableSteam ResistantHigh Flow | |||
| Processing | Injection | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Melt Mass Flow Rate(MFR) | |||
230°C/2.16 kg | *** g/10min | ISO 1133 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-2 | 1 mm/min |
Tensile Strength | |||
Yield | *** Mpa | ISO 527-2 | 50 mm/min |
Tensile Elongation | |||
Yield | *** % | ISO 527-2 | 50 mm/min |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-2 | |
Vicat Softening Temperature(VST) | *** °C | ISO 306 | 10 N |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.