ICORENE® 3550 is a linear low density polyethylene for rotational molding applications. The grade is UV stabilized and suitable for applications requiring good stiffness and processability.
| Original Document | Technical Datasheet-ASTM(English) | |||
| Features | Good StiffnessEasy processingUV Stabiltiy | |||
| Additive | UV-Stabilizer | |||
| Appearance | PowderNatural Color | |||
| Processing | Rotational Molding | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | ***~*** g/cm³ | ASTM D 1505 | |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | ***~*** g/10min | ASTM D1238 | |
Environmental Stress Cracking Resistance | *** Hours | ASTM D 1693 | 100% Igepal, F50 |
Environmental Stress Cracking Resistance | *** Hours | ASTM D 1693 | Condition A, 10% Igepal, F50 |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ASTM D638 | 51 mm/min, Rotational Molded |
Tensile Elongation | |||
Break | *** % | ASTM D638 | 51 mm/min, Rotational Molded |
Flexural Modulus | *** Mpa | ASTM D790 | 1% Secant, Rotational Molded |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Falling Dart Impact | *** J | Internal | -40°C, 3.18 mm, Rotational Molded |
Falling Dart Impact | *** J | Internal | -40°C, 6.35 mm, Rotational Molded |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ASTM D648 | Unannealed, Rotational Molded |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ASTM D648 | Unannealed |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.