Xenoy product that provides improved chemical resistance and impact performance versus previous generation X2202 product which is used in the market spaces such as soap dispenser, cleaning equipment, filter housing
| Original Document | Technical Datasheet(English) | |||
| Features | High ImpactChemical Resistance | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Melt Volume Flow Rate(MVR) | |||
265°C/5.0 kg | *** cm³/10 min | ISO 1133 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Flexural Modulus | *** Mpa | ASTM D790 | 1.3 mm/min, 50 mm span |
Flexural Strength | |||
Yield | *** Mpa | ASTM D790 | 1.3 mm/min, 50 mm span |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Izod Notched Impact Strengh | |||
-20℃ (-4℉) | *** J/m | ASTM D256 | |
0℃ (32℉) | *** J/m | ASTM D256 | |
23℃ (73℉) | *** J/m | ASTM D256 | |
Instrumented Impact Energy | |||
-20℃ (-4℉) Total Energy | *** J | ASTM D3763 | |
0℃ (32℉)Total Energy | *** J | ASTM D 3763 | |
23℃ (73℉)Total Energy | *** J | ASTM D3763 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ASTM D648 | 3.2 mm, unannealed |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ASTM D648 | 3.2 mm, unannealed |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.