Developmental Grade-Terpolymer with low SIT for skin layer of CPP and BOPP films.
Features
Low sealing initial temperature
High transparency and high gloss
Barefoot formulation for sealing layer
Excellent processing on high speed equipment
Applications
Skin layer of co-extruded CPP and BOPP films
| Original Document | Technical Datasheet-ASTM(English) | |||
| Features | Light TransmissionHigh Gloss | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Melt Mass Flow Rate(MFR) | |||
230°C/2.16 kg | *** g/10min | ASTM D 1238 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Yield | *** Mpa | ASTM D638 | |
Tensile Elongation | |||
Yield | *** % | ASTM D638 | |
Flexural Modulus | *** Mpa | ASTM D790 | |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Izod Notched Impact Strengh | |||
23℃ (73℉) | *** J/m | ASTM D256 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ASTM D648 | |
| Optical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Haze | *** % | ASTM D1003 | |
Gloss | *** % | ASTM D 2457 | |
| Film | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Seal Initiation Temperature | *** °C | Internal |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.