Zytel® HTNFR52G30BL NC010 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.
| Original Document | Technical Datasheet-ISO(Chinese) | |||
| Features | Flame RetardantFilled & Reinforced | |||
| Reinforced | 30% Glass Fiber | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** kg/m³ | ISO 1183 | |
Molding Shrinkage | |||
Flow | *** % | ISO 294-4, 2577 | |
Across Flow | *** % | ISO 294-4, 2577 | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Modulus | *** Mpa | ISO 527-1/-2 | |
Tensile Modulus | *** Mpa | ISO 527-1/-2 | Conditioned |
Tensile Strength | |||
Break | *** Mpa | ISO 527-1/-2 | |
Break | *** Mpa | ISO 527-1/-2 | Conditioned |
Tensile Elongation | |||
Break | *** % | ISO 527-1/-2 | |
Break | *** % | ISO 527-1/-2 | Conditioned |
Flexural Modulus | *** Mpa | ISO 178 | |
Flexural Strength | |||
- | *** Mpa | ISO 178 | |
- | *** Mpa | ISO 178 | Conditioned |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Charpy Notched Impact Strengh | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | |
Charpy Unnotched Impact Strengh | |||
-40℃ (-40℉) | *** kJ/m² | ISO 179/1eU | |
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | |
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | Conditioned |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Conditioned |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Heat Deflection Temperature(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75-1/-2 | |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75-1/-2 | |
Relative Temperature Index(RTI), Imp | |||
1.5/1.6 mm | *** °C | UL 746B | |
3.0/3.2 mm | *** °C | UL 746B | |
Relative Temperature Index(RTI), Elec | |||
1.5/1.6 mm | *** °C | UL 746B | |
3.0/3.2 mm | *** °C | UL 746B | |
Relative Temperature Index(RTI), Str | |||
1.5/1.6 mm | *** °C | UL 746B | |
3.0/3.2 mm | *** °C | UL 746B | |
Coefficient of Linear Thermal Expansion | |||
Flow | *** E-6/K | ISO 11359-1/-2 | |
Flow | *** E-6/K | ISO 11359-1/-2 | -40-23℃ |
Flow | *** E-6/K | ISO 11359-1/-2 | 55-160℃ |
Across Flow | *** E-6/K | ISO 11359-1/-2 | |
Across Flow | *** E-6/K | ISO 11359-1/-2 | -40-23℃ |
Across Flow | *** E-6/K | ISO 11359-1/-2 | 55-160℃ |
Melt Temperature(Tm) | *** °C | ISO 11357-1/-3 | |
| Flammability | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Flame Rating | |||
V-0 | *** mm | UL94 | |
V-0 | *** mm | UL94 | |
5VA | *** mm | UL94 | |
Oxygen Index | *** % | ISO 4589-1/-2 | |
Glow Wire Flammability Index(GWFI) | |||
0.75mm | *** °C | IEC 60695-2-12 | |
1.5mm | *** °C | IEC 60695-2-12 | |
3mm | *** °C | IEC 60695-2-12 | |
Glow Wire Ignition Test(GWIT) | |||
0.75mm | *** °C | IEC 60695-2-13 | |
1.5mm | *** °C | IEC 60695-2-13 | |
3.0mm | *** °C | IEC 60695-2-13 | |
FMVSS | *** - | FMVSS 302 | |
| Electrical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Volume Resistivity | *** Ohm-m | IEC 60093 | |
Dielectric Constant(Permittivity) | |||
100Hz | *** - | IEC 60250 | |
1MHz | *** - | IEC 60250 | |
Dissipation Factor | |||
100Hz | *** E-4 | IEC 60250 | |
1MHz | *** E-4 | IEC 60250 | |
Comparative Tracking Index (CTI) | |||
- | *** - | IEC 60112 | |
- | *** - | IEC 60112 | M |
- | *** PLC | UL 746A | |
Dielectric Strength | *** kV/mm | IEC 60243-1 | |
| Additional Information | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Fogging | |||
F-value (refraction) | *** % | ISO 6452 | |
Odor test | *** class | VDA 270 |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.