LOTADER® 3210 is a random terpolymer of ethylene, acrylic ester and maleic anhydride, polymerized by high-pressure autoclave process.
Applications
LOTADER® 3210 is a versatile adhesive for extrusion coating or lamination, designed as :
Concentrate to be used in dry blend with LDPE. LOTADER® 3210 improves adhesion of LDPE on aluminium foils, metallized or primerized films.
Ready for use resin to be used pure. LOTADER® 3210 gives excellent adhesion on substrates likes aluminium foil, metallized plastics, paper, board, PE and some plastic films like BOPP.
Coextrusion tie layer for PE/PA in extrusion coating process.
LOTADER® 3210 is also a coupling agent for mineral filled compounds such as halogen free flame retardant wires and cables, a compatibilizer for polyamide/polyolefin blends and a modifier for polyamides.
| Original Document | Technical Datasheet(English) | |||
| Features | Good Adhesion | |||
| Appearance | Pellets/Granules | |||
| Processing | ExtrusionCo-extrusionLaminationExtrusion CoatingCompounding | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ISO 1183 | |
Melt Mass Flow Rate(MFR) | |||
190℃/2.16 kg | *** g/10min | ISO 1133 | |
Maleic Anhydride Content | *** % | Internal | |
Butyl Acrylate Content | *** % | Internal | |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
Break | *** Mpa | ISO 527-2 | |
Tensile Elongation | |||
Break | *** % | ISO 527-2 | |
Flexural Modulus | *** Mpa | ISO 178 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore D hardness | *** D | ISO 868 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Vicat Softening Temperature(VST) | *** °C | ISO 306 | 10N |
Melt Temperature(Tm) | *** °C | ISO 11357-3 |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.