Texin 990 resin is a polyether-based thermoplastic polyurethane with a Shore hardness of approximately 90A. It can be processed by injection molding, extrusion, or blow molding.
Texin 990 resin offers outstanding abrasion resistance, impact strength, toughness, and flexibility. It also exhibits excellent inherent resistance to salt water stress cracking, and hydrolysis. Texin 990 natural color resin complies with FDA food-contact regulations 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber Articles Intended for Repeated Use), subject to the limitations of these and any other applicable regulations. In addition, Texin 990 natural color resin is listed under NSF standard 61 for use in potable water applications. Typical applications include belting, hose, seals and gaskets, tubing, cable and hose jackets, athletic soles, casters, film, extruded profiles and miscellaneous molded articles. As with any product, use of Texin 990 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.
| Original Document | Technical Datasheet(English) | |||
| Features | High ImpactGood ToughnessWear/Abrasion ResistanceFood ContactDrinking Water ContactHydrolysis ResistanceChlorid(CaCl2/Salt)Resitance | |||
| Processing | InjectionExtrusionBlow Molding | |||
| Compliance | FDANSF | |||
| Physical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
|---|---|---|---|
Density/Specific Gravity | *** g/cm³ | ASTM D792 | |
Mold Shrinkage | |||
Flow | *** % | ASTM D955 | 2.54 mm |
Across Flow | *** % | ASTM D955 | 2.54 mm |
Abrasion resistance | *** mg/1000cy | ASTM D 3489 | H-18, 1,000-g Load |
| Mechanical | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Tensile Strength | |||
- | *** Mpa | ASTM D 412 | |
at 50% strain | *** Mpa | ASTM D 412 | |
at 100% strain | *** Mpa | ASTM D 412 | |
at 300% strain | *** Mpa | ASTM D 412 | |
Tensile Elongation | |||
Break | *** % | ASTM D 412 | |
Flexural Modulus | *** Mpa | ASTM D790 | 73°F (23°C) |
Tear Strength | *** kN/m | ASTM D 624 | Die C |
Compression Set | *** % | ASTM D 395 | 22 Hours at 158°F (70°C) |
Compression Set | *** % | ASTM D 395 | 22 Hours at 73°F (23°C) |
Compression Set | *** % | ASTM D 395 | Postcured, 22 Hours at 158°F (70°C) |
Compression Set | *** % | ASTM D 395 | Postcured, 22 Hours at 73°F (23°C) |
Compressive Strength | *** Mpa | ASTM D 575 | 10% Deflection |
Compressive Strength | *** Mpa | ASTM D 575 | 15% Deflection |
Compressive Strength | *** Mpa | ASTM D 575 | 2% Deflection |
Compressive Strength | *** Mpa | ASTM D 575 | 20% Deflection |
Compressive Strength | *** Mpa | ASTM D 575 | 25% Deflection |
Compressive Strength | *** Mpa | ASTM D 575 | 5% Deflection |
Compressive Strength | *** Mpa | ASTM D 575 | 50% Deflection |
Rebound Resilience | *** % | ASTM D 2632 | Bayshore Resilience |
| Impact | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Brittleness Temperature | *** °C | ASTM D 746 | |
| Hardness | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Shore A hardness | *** A | ASTM D 2240 | |
| Thermal | Value/Unit(Sign in to View) | Test Standard | Test Condition |
Vicat Softening Temperature(VST) | *** °C | ASTM D1525 | Rate A |
Glass Transition Temperature | *** °C | Internal |
The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.