Reinforced, filled and flame-retardant VESTAMID® polyamide 12 compounds
Characterization: low viscosity, with flame retardant, halogen and phosphorus-free, UL94-V0/V2, with processing aid
Applications: wire insulation
• Lowest water absorption of all commercially available polyamides. As a result, the properties vary little and molded parts exhibit almost no dimensional changes with variations in humidity.
• Extraordinarily high impact resistance and notched impact strength – immediately after injection molding and also well below the freezing point
• Good to very good resistance to greases,oils, fuels, hydraulic fluids, and many solvents as well as to salt solutions, etc.
• Excellent resistance to stress cracking, even for metal parts encapsulated by injection molding or embedded
• Excellent abrasion resistance
• Low coefficient of sliding friction, in dry running against steel, polybutylene terephthalate, polyacetal and other materials
• Noise and vibration damping properties
• Excellent resistance to fatigue caused by frequent load change
• High processability
| 原厂资料 | 物性表(英文) | |||
| 缩写标识 | PA12 FR(30) | |||
| 产品特性 | 耐疲劳高冲击耐低温冲击阻燃无卤无红磷耐磨低摩擦食品接触级ESCR耐氯(氯化钙/盐)耐燃油耐油耐溶剂低粘度降噪音阻尼减震 | |||
| 添加助剂 | 阻燃剂加工助剂 | |||
| 颜色形状 | 粒状本色 | |||
| 成型方式 | 注塑挤出 | |||
| 法规认证 | EU 2011/10/EC (欧盟食品级)FDA(食品药品监督管理局) | |||
| 曲线坐标点 | 比容-温度(pvT) | |||
| 物理性能 | 值/单位(登录后可见) | 测试标准 | 测试条件 |
|---|---|---|---|
密度 | *** g/cm³ | ISO 1183 | |
收缩率 | |||
纵向(Flow) | *** % | ISO 294-4 | |
横向(Across Flow) | *** % | ISO 294-4 | |
吸水率 | *** % | ISO 62 | 23°C, 50% relative humidity |
吸水率 | *** % | ISO 62 | 23°C, saturation |
| 机械性能 | 值/单位(登录后可见) | 测试标准 | 测试条件 |
拉伸模量 | *** Mpa | ISO 527-1/-2 | |
拉伸强度 | |||
屈服(yld) | *** Mpa | ISO 527-1/-2 | |
拉伸延伸率 | |||
屈服(yld) | *** % | ISO 527-1/-2 | |
断裂(brk) | *** % | ISO 527-1/-2 | |
| 冲击性能 | 值/单位(登录后可见) | 测试标准 | 测试条件 |
简支梁缺口(Charpy Notched) | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eA | Complete break |
23℃ (73℉) | *** kJ/m² | ISO 179/1eA | Complete break |
简支梁无缺口(Charpy Unnotched) | |||
-30℃ (-22℉) | *** kJ/m² | ISO 179/1eU | Complete break |
23℃ (73℉) | *** kJ/m² | ISO 179/1eU | Complete break |
| 热学性能 | 值/单位(登录后可见) | 测试标准 | 测试条件 |
热变形温度(HDT) | |||
0.45 Mpa (66 psi)(4.6kg/cm²) | *** °C | ISO 75 | |
1.8 Mpa (264 psi)(18.6kg/cm²) | *** °C | ISO 75 | |
维卡软化温度(Vicat) | *** °C | ISO 306 | 10 N |
维卡软化温度(Vicat) | *** °C | ISO 306 | 50 N |
熔融温度(Tm) | *** °C | ISO 11357 | DSC, 2nd heating |
| 燃烧性能 | 值/单位(登录后可见) | 测试标准 | 测试条件 |
防火等级 | |||
V-2 | *** mm | UL94 | |
V-2 | *** mm | UL94 | |
| 电学性能 | 值/单位(登录后可见) | 测试标准 | 测试条件 |
体积电阻率 | *** Ohm-cm | IEC 60093 | |
介电常数(DK) | |||
1MHz | *** - | IEC 60250 | 23°C |
耗散因数(DF) | |||
1MHz | *** E-4 | IEC 60250 | 23°C |
相对漏电起痕指数(CTI ) | |||
溶液A | *** V | IEC 60112 | |
溶液A | *** V | IEC 60112 | 100 drops value |
绝缘强度 | *** kV/mm | IEC 60243-1 | K20/P50 |
此物性表中的信息由阿技材料库从该材料的生产商处获得。阿技材料库尽最大努力确保此数据的准确性。 但是阿技材料库对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。