Grilamid® L 25 G nat 6011

PA12

EMS-GRIVORY

Product Description

Processing

Other Extrusion

Delivery form

Granules

Regional Availability

North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Product Attributes

High viscosity

Packaging

Non oriented film

Food Contact

EU Requirements, FDA

General
Original Document
Technical Datasheet(English)
Technical Datasheet(Chinese)
Features
Food Contact
High Viscosity
Appearance
Pellets/Granules
Natural Color
Processing
Extrusion
Film Extrusion
Compliance
EU 2011/10/EC
FDA
Specifications
Physical Value/Unit(Sign in to View) Test Standard Test Condition

Density/Specific Gravity

*** g/cm³ ISO 1183
dry

Melt Volume Flow Rate(MVR)

275°C/5 kg

*** cm³/10 min ISO 1133
dry

Water Absorption

*** % ISO 62
dry

Moisture /Humidity Absorption

*** % ISO 62
dry
Mechanical Value/Unit(Sign in to View) Test Standard Test Condition

Tensile Modulus

*** Mpa ISO 527-1/-2
cond.

Tensile Modulus

*** Mpa ISO 527-1/-2
dry
Impact Value/Unit(Sign in to View) Test Standard Test Condition

Charpy Notched Impact Strengh

-30℃ (-22℉)

*** kJ/m² ISO 179/1eA
cond.

23℃ (73℉)

*** kJ/m² ISO 179/1eA
cond.
Thermal Value/Unit(Sign in to View) Test Standard Test Condition

Melt Temperature(Tm)

*** °C ISO 11357-1/-3
dry

Continuous Use Temperature

Long term

***~*** °C ISO 2578
long term

Temperature at Short Circle Operation

*** °C Internal
short term
Optical Value/Unit(Sign in to View) Test Standard Test Condition

Gloss

*** - ISO 2813
dry, 60°
Film Value/Unit(Sign in to View) Test Standard Test Condition

Tensile Strength

Yield

*** Mpa ISO 527-3
dry, normal

Yield

*** Mpa ISO 527-3
dry, parallel

Break

*** Mpa ISO 527-3
dry, normal

Break

*** Mpa ISO 527-3
dry, parallel

Tensile Elongation

Yield

*** % ISO 527-3
dry, normal

Yield

*** % ISO 527-3
dry, parallel

Break

*** % ISO 527-3
dry, normal

Break

*** % ISO 527-3
dry, parallel

Gelbo Flex Testing

*** holes/m² company
dry

Elmondorf Tear

*** N ISO 6383-2
dry, normal

Elmondorf Tear

*** N ISO 6383-2
dry, parallel

Trouser Tear

*** kN/m ISO 6383-1
dry, normal

Trouser Tear

*** kN/m ISO 6383-1
dry, parallel

Water Vapor Transmission Rate

*** g/m²/24 hr ISO 15106-1/-2
dry, 23°C/85%r.h.

Oxygen permeability

*** cm³/m²/bar/24 hr DIS 15105-1/-2
dry, 23°C/0%r.h.

Oxygen permeability

*** cm³/m²/bar/24 hr DIS 15105-1/-2
dry, 23°C/85%r.h.

Carbon Dioxide transm. rate

*** cm³/m²/bar/24 hr ISO 15105-1/-2
dry, 23°C/0%r.h.

Carbon Dioxide transm. rate

*** cm³/m²/bar/24 hr ISO 15105-1/-2
dry, 23°C/85%r.h.

The information presented on this datasheet was acquired by AjiEng.com from the producer of the material. AjiEng.com makes substantial efforts to assure the accuracy of this data. However, AjiEng.com assumes no responsibility for the data values and strongly encourages that upon final material selection, data points are validated with the material supplier.